Low Density Polyethylene 2420H

PropertyTest methodUnitvalue
DensityISO 1183g/cm³0.924
Melt flow rate (MFR) (190°C/2.16kg)ISO 1133g/10 min1.9
Melt flow rate (MFR) (190°C/2.16kg)ASTM D 1709g110
Tensile ModulusISO 527-1, -2Mpa260
Tensile Stress at YieldISO 527-1, -2Mpa11.0
Tensile Strength MD TDISO 527-1, -3Mpa
Mpa
25.0 21.0
Tensile strengthat Break MD TDISO 527-1, -3% %250 600
Vicat softening temperature (A50 (50°C/h 10N))ISO 306°C94.0
Melting TemperatureISO 3146°C111
Haze (50ìm)ASTM D 1003%<8
Gloss (20°, 50ìm) (60°, 50ìm)ASTM D 2457>15 >50
Melt Temperature-°C160 to 200
Film properties tested using 50 ìm thickness blown film extruded at a melt temperature of 180°C and a blow-up ratio of 1:2.5
Failure Energy, 70ìmDIN 53373J/mm4
Coefficient of FrictionISO 8295%>80
Recommended Thickness-ìm20 to 100